Colemanite AM

Alternate Names: Calcium Borate

Oxide Analysis Formula Tolerance
B2O3 46.00% 1.29
CaO 28.00% 0.97
SiO2 3.00% 0.10
MgO 0.60% 0.03
LOI 17.00%n/a
Oxide Weight 150.97
Formula Weight 181.90

Notes

The chemistry shown appears to be incomplete.

Related Information

Links

Materials Colemanite
A natural source of boron that melts at a very low temperature.
Typecodes Flux Source
Materials that source Na2O, K2O, Li2O, CaO, MgO and other fluxes but are not feldspars or frits. Remember that materials can be flux sources but also perform many other roles. For example, talc is a flux in high temperature glazes, but a matting agent in low temperatures ones. It can also be a flux, a filler and an expansion increaser in bodies.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy