Champion-Challenger

Alternate Names: Champion Challenger Ball Clay, Chalenger

Description: 1/2 Champion, 1/2 Challenger

Oxide Analysis Formula Tolerance
CaO 0.37% 0.02
K2O 0.40% 0.02
MgO 0.30% 0.03
Na2O 0.12% 0.01
TiO2 1.64% 0.07
Al2O3 28.38% 1.00
P2O5 0.15% -
SiO2 55.60% 3.32
Fe2O3 0.98% 0.02
MnO 0.02% -
LOI 12.30%n/a
SO3 0.03%n/a
Oxide Weight 316.14
Formula Weight 360.60

Notes

Relative Viscosity (1.2 Sp. Gr.):* 1.53
Casting Rate: (gms per 15 min/426 cm2):* 177
Water of Plasticity:* 23.6
% Dry Shrinkage:* 5.86
Dry M.O.R., psi:* 700

Cone 04 8 11
----
Fired Shrinkage:* 0.3% 2.1% 2.5%
Absorption:* 18.7% 15.5% 15.1%
M.O.R. psi:* 1720 4100 3860

Thermal Expansion, Cone 8: 0.51% at 700C
P.C.E.: 33
pH: 5.5
Oil Absorption: 38
Bulk Density, lbs per cubic foot: 33-38
Particle Size, Microns: 20 10 5 2 1 0.5 0.2
97% 94% 86% 75% 64% 47% 16%

*Specimens: De-aired, extruded, 50% ball clay, 50% flint

Related Information

Links

Typecodes Ball Clay
Ball clays are abundant and very plastic and are used in all types of plastic forming bodies. They are not as white-burning or refractory as kaolins but lower in iron and fluxes than bentonites.
Materials Champion Ball Clay

Data

Pyrometric Cone Equivalent 33

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy