1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Champion Ball Clay

Description: For sanitary and dinner ware

Oxide Analysis Formula Tolerance
CaO 0.40% 0.03
K2O 0.40% 0.02
MgO 0.30% 0.03
Na2O 0.15% 0.01
TiO2 1.60% 0.07
Al2O3 28.40% 1.00
P2O5 0.15% -
SiO2 55.60% 3.32
Fe2O3 1.00% 0.02
LOI 12.00%n/a
Oxide Weight 316.06
Formula Weight 359.15

Notes

The manufacturer describes it as a fine grained blend producing excellent strength with good fired whiteness.

Related Information

Links

Typecodes Ball Clay
Ball clays are abundant and very plastic and are used in all types of plastic forming bodies. They are not as white-burning or refractory as kaolins but lower in iron and fluxes than bentonites.
Materials Champion-Challenger

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy