1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Ceramitalc HDT

Oxide Analysis Formula Tolerance
CaO 8.71% 0.17
MgO 29.60% 0.82
Na2O 0.34% 0.01
Al2O3 0.36% -
SiO2 55.86% 1.04
Fe2O3 0.17% -
MnO 0.12% -
LOI 4.84%n/a
Oxide Weight 106.30
Formula Weight 111.70

Notes

No longer available.

A pressing grade of talc used in ceramic wall tile and artware. It develops high thermal expansion and low moisture expansion to prevent crazing in bodies that can be safety fired at rapid cycles.

Related Information

Links

Materials Talc
A source of MgO for ceramic glazes, a flux or thermal expansion additive in clay bodies, also used in the manufacture of cordierite.
Materials Ceramitalc
Typecodes Flux Source
Materials that source Na2O, K2O, Li2O, CaO, MgO and other fluxes but are not feldspars or frits. Remember that materials can be flux sources but also perform many other roles. For example, talc is a flux in high temperature glazes, but a matting agent in low temperatures ones. It can also be a flux, a filler and an expansion increaser in bodies.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.