1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Ceramelt

Alternate Names: Ground glass terra cotta, brick, roof tile body flux

Notes

This material is added to terra cotta bodies to improve maturity and fired strength. The manufacturer claims that a 5% addition can reduce energy costs by 15% accompanied by a significant improvement in strength and resistance to freeze-thaw failure.

Related Information

Links

Oxide Analysis Formula Tolerance
Typecodes Flux Source
Materials that source Na2O, K2O, Li2O, CaO, MgO and other fluxes but are not feldspars or frits. Remember that materials can be flux sources but also perform many other roles. For example, talc is a flux in high temperature glazes, but a matting agent in low temperatures ones. It can also be a flux, a filler and an expansion increaser in bodies.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy