1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Caolín Blanco (Cuba)

Description: Cuban kaolin

Oxide Analysis Formula Tolerance
SiO2 45.20% 1.99
Al2O3 38.50% 1.00
Fe2O3 0.73% 0.01
TiO2 0.95% 0.03
CaO 0.55% 0.03
MgO 0.77% 0.05
K2O 1.70% 0.05
Na2O 0.77% 0.03
LOI 11.60%n/a
Oxide Weight 236.24
Formula Weight 267.24

Related Information

Links

Materials Kaolin
The purest of all clays in nature. Kaolins are used in porcelains and stonewares to impart whiteness, in glazes to supply Al2O3 and to suspend slurries.
Materials Arcilla de Pontezuelo (Cuba)
Materials Caolín Gris (Cuba)
Materials Caolín Mantua (Cuba)
Materials Caolín Damanueco (Cuba)
Materials Caolín Santa Elena (Cuba)
Typecodes Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy