Description: Cuban clay
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| SiO2 | 64.80% | 4.69 | |
| Al2O3 | 23.45% | 1.00 | |
| Fe2O3 | 0.42% | 0.01 | |
| TiO2 | 0.65% | 0.04 | |
| CaO | 0.39% | 0.03 | |
| MgO | 0.63% | 0.07 | |
| K2O | 2.07% | 0.10 | |
| Na2O | 0.37% | 0.03 | |
| LOI | 6.44% | n/a | |
| Oxide Weight | 403.56 | ||
| Formula Weight | 431.34 | ||
| Materials |
Barro Ovas (Cuba)
|
| Materials |
Arcilla Club de Cazadores (Cuba)
|
| Materials |
Arcilla Revolucion III (Cuba)
|
| Materials |
Arcilla Revolucion II (Cuba)
|
| Materials |
Arcilla Revolucion I (Cuba)
|
| Materials |
Caolín Santa Elena (Cuba)
|
| Materials |
Caolín Damanueco (Cuba)
|
| Materials |
Caolín Mantua (Cuba)
|
| Materials |
Caolín Blanco (Cuba)
|
| Materials |
Caolín Gris (Cuba)
|
| Materials |
Ciego de Avila (Cuba)
|
| Typecodes |
Clay Other
Clays that are not kaolins, ball clays or bentonites. For example, stoneware clays are mixtures of all of the above plus quartz, feldspar, mica and other minerals. There are also many clays that have high plasticity like bentonite but are much different mineralogically. |
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
| By Tony Hansen Follow me on ![]() | ![]() |
Buy me a coffee and we can talk