Description: ANTIMONATE OF LEAD
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| PbO | 66.40% | 1.00 | |
| Sb2O3 | 29.40% | 0.34 | |
| LOI | 4.20% | n/a | |
| Oxide Weight | 322.03 | ||
| Formula Weight | 336.14 | ||
A creamish yellow powder used to introduce antimony into Naples yellow lead glazes. During melting and dissolution, oxygen is liberated to convert Sb2O5 to Sb2O3.
| Typecodes |
Flux Source
Materials that source Na2O, K2O, Li2O, CaO, MgO and other fluxes but are not feldspars or frits. Remember that materials can be flux sources but also perform many other roles. For example, talc is a flux in high temperature glazes, but a matting agent in low temperatures ones. It can also be a flux, a filler and an expansion increaser in bodies. |
| Frit Softening Point | 800C |
|---|