Kamogawa Stone

Oxide Analysis Formula Tolerance
CaO 5.98% 0.43
K2O 1.19% 0.05
MgO 3.01% 0.30
Na2O 3.41% 0.22
TiO2 2.24% 0.11
Al2O3 13.94% 0.55
SiO2 54.79% 3.66
Fe2O3 13.24% 0.33
LOI 2.19%n/a
Oxide Weight 392.90
Formula Weight 401.70

Notes

We do not know much about this material, and have lost track of where this analysis is from. However, if this chemistry is correct, this is clearly a well fluxed material that would melt well. It also has an exceptionally high iron content not to mention alot of TiO2.

A potter from Japan told us that the glaze on black Raku tea bowls was made from Kamogawa stone and that they included lead.


PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy