Description: Harcros easy dispersing yellow iron oxide
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Fe2O3 | 88.00% | 1.00 | |
| LOI | 12.00% | n/a | |
| Oxide Weight | 160.00 | ||
| Formula Weight | 181.82 | ||
Harcros makes two types of yellow iron; Easy Dispersing and Regular. Both are 99.9% minus 325 mesh and have 85%+ Fe2O3. The former consists of five products ranging from light shade YLO-1888D to deep shade YLO-4088D. These products offer closely controlled mass color, tint, and strength combined with easy dispersion properties.
The regular grade consists of six products from light yellow YO-2087 to deep yellow YO-8087 (density increases and surface area decreases dramatically across this range).
The Hegman values of the regular material are not as high. The products will withstand temperatures to 450-500F in most vehicle systems. They are non-fading and non-reactive in weak acids and alkalis. They are ideal as colorants in paints, enamels, concrete, plastic, rubber and paper.
| Materials |
Iron Oxide Black
|
| Materials |
Spanish Red Iron Oxide
|
| Materials |
Natural Red Iron Oxide
|
| Materials |
Mapico 1075A Yellow Iron Oxide
|
| Typecodes |
Colorant
Metallic based materials that impart fired color to glazes and bodies. |
| Density (Specific Gravity) | 4.03 |
|---|---|
| pH for dry powder | 7.0 |
| By Tony Hansen Follow me on ![]() | ![]() |