Spanish Red Iron Oxide

Oxide Analysis Formula Tolerance
Fe2O3 87.00% 1.00
SiO2 5.00% 0.15
Oxide Weight 169.20
Formula Weight 169.20

Notes

Some suppliers claim that Crocus Martis and Spanish Red Iron are the same. However this material is said to be a very bright orange when raw and it is not the same. If you know more about this material, please let us know. It appears to be from Tierga Mines, the Santa Rosa mine in Zaragoza-Aragón, Spain. The deposit appears to be layered with dolomite (thus the unaccounted for 8%).
The material has some soluble salts (0.1% or more).

Tom Buck said this: "In Spain, there exists one large ore body assaying low amounts of iron sulfide (mostly), too inadequate for steel-making even with modern "float sink" technology. Long ago, however, an astute person noticed that rainwater would pool, then evaporate and leave behind a mineral that turned red on roasting. In time, it was discovered that a specific life-form (a bacterium, named bacillus ferro ferroxidans) used the iron sulfide as food (an energy source). The bacterium did its thing in water in contact with the iron mineral. The result is to solubilize the iron as Iron(II) Sulfate or FeSO4. This solution is run into evaporation ponds, the green crystals recovered are then roasted to form Spanish red (iron oxide red). To keep costs as low as possible, the mine operators in Spain are happy with an Iron Oxide Red purity that ranges from 83 to 88 percent by weight. If you as a potter were able to obtain Spanish Red as such bag after bag, then you'd tweak your recipes to get the best glaze colour."

Related Information

Links

Materials Crocus Martis
Materials Iron Sulfate
Materials Iron Oxide Red
Red iron oxide is the most common colorant used in ceramic bodies and glazes. As a powder, it is available in red, yellow, black and other colors.
Materials Iron Oxide Black
Materials YLO-1888D Yellow Iron Oxide
Materials Iron Oxide Yellow
URLs http://www.igme.es/internet/PanoramaMinero/actual/OXHIER08.pdf
Document from Tierga Mines about Spanish iron oxides

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy