Mapico 1075A Yellow Iron Oxide

Alternate Names: Pigment Yellow 42

Description: Ferric Oxide Hydrate

Formula: FeOOH

Oxide Analysis Formula Tolerance
Fe2O3 87.00% 1.00
H2O 12.00%n/a
Oxide Weight 160.00
Formula Weight 181.82

Notes

Manufacturer using the Martin process.
Typical trace elements ppm: As < 1, Sb < 8, Cd < 1, Cr < 5, Cu < 1, Pb < 3, Hg < 0.1, Ni < 150, Se < .5

Related Information

Links

Materials YLO-1888D Yellow Iron Oxide
Typecodes Colorant
Metallic based materials that impart fired color to glazes and bodies.

Data

% Passing 325 Mesh Wet .02
Density (Specific Gravity) 4.1
pH for dry powder 6.5

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy