Monthly Tech-Tip from Tony Hansen SignUp

No tracking! No ads!

1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Pemco Frit P-586

Alternate Names: Frit 586, Frit P586

Description: Barium, zinc, calcium frit for partially fritted cone 4-10 glazes

Oxide Analysis Formula Tolerance
BaO 4.10% 0.05
CaO 14.30% 0.48
K2O 4.00% 0.08
MgO 0.60% 0.03
Na2O 1.60% 0.05
ZnO 13.40% 0.31
B2O3 4.50% 0.12
Al2O3 8.20% 0.15
SiO2 49.30% 1.55
Oxide Weight 188.88
Formula Weight 188.88

Related Information

Links

Materials Fusion Frit FZ-22
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit 3276
Materials Hommel Frit 1030
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 7.30
Co-efficient of Linear Expansion 7.5 x 10-6 (50-450C)
Frit Melting Range (C) 1600-1860F
I.F.P. (celsius) 689C