Pemco Frit P-311

Alternate Names: Frit 311, Frit P311

Description: Calcium borosilicate frit for partially fritted dinnerware glazes

Oxide Analysis Formula Tolerance
CaO 14.10% 0.69
K2O 0.70% 0.02
Na2O 6.50% 0.29
B2O3 14.40% 0.57
Al2O3 10.00% 0.27
SiO2 54.30% 2.48
Oxide Weight 275.02
Formula Weight 275.02

Related Information

Links

Materials Fusion Frit F-19
A commonly available calcium borosilicate frit having a similar chemistry to Ferro Frit 3124.
Materials Hommel Frit 378A
Materials Ferro Frit 3124
A commonly available calcium borosilicate frit.
Materials Hommel Frit 90
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials General Frit GF-113
Materials Pemco Frit P-2N87
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 7.0 x 10-6 (50-450C)
Frit Melting Range (C) 1500-1630F
I.F.P. (celsius) 669C