Pemco Frit P-2N87

Alternate Names: 2N87,2N-87

Description: High alkali, low alumina, low boron leadless frit

Notes

Modification of P-311 used in same manner

Related Information

Links

Oxide Analysis Formula Tolerance
Materials Pemco Frit P-311
Typecodes Frit