Pemco Frit P-1N72

Alternate Names: 1N-72,1N72

Description: Alkali-alumina-borosilicate body frit

Oxide Analysis Formula Tolerance
K2O 1.80% 0.07
Na2O 15.80% 0.93
B2O3 24.00% 1.26
Al2O3 3.90% 0.14
SiO2 54.50% 3.31
Oxide Weight 365.03
Formula Weight 365.03

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Fusion Frit F-74
Materials Hommel Frit 4GF153A
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 9.30
Co-efficient of Linear Expansion 9.30 (50-450C)
Frit Softening Point 1400F
Frit Melting Range (C) 1350-1450F
Co-efficient of Linear Expansion 9.3x10-6 (50-450C)
I.F.P. (celsius) 587C