Fusion Frit F-74

Alternate Names: Fusion Frit F74

Description: Alkaline boron flux

Oxide Analysis Formula Tolerance
K2O 1.40% 0.05
Na2O 16.00% 0.95
B2O3 24.00% 1.26
Al2O3 4.00% 0.14
SiO2 54.60% 3.33
Oxide Weight 366.40
Formula Weight 366.40

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Pemco Frit P-1N72
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 7.91 x 10-6
Frit Softening Point 1450F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy