Pemco Frit P-1F07

Alternate Names: 1F07,1F-07

Description: High CaO/Na2O/ZnO borosilicate low alumina frit

Oxide Analysis Formula Tolerance
BaO 3.70% 0.04
CaO 14.30% 0.44
K2O 1.10% 0.02
MgO 0.40% 0.02
Na2O 9.60% 0.27
ZnO 9.70% 0.21
Sb2O3 0.10% -
B2O3 20.20% 0.51
Al2O3 4.30% 0.07
SiO2 36.10% 1.05
Oxide Weight 173.15
Formula Weight 173.15

Notes

For partially-fritted textured glazes.

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 9.30
Co-efficient of Linear Expansion 9.30 (50-450C)
Frit Softening Point 1450F
Frit Melting Range (C) 1380-1540F
Co-efficient of Linear Expansion 9.5x10-6 (50-450C)
I.F.P. (celsius) 690C
By Tony Hansen