| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| BaO | 2.84% | 0.05 | |
| CaO | 11.01% | 0.55 | |
| K2O | 0.04% | - | |
| MgO | 0.45% | 0.03 | |
| Na2O | 8.26% | 0.37 | |
| B2O3 | 16.23% | 0.65 | |
| Al2O3 | 6.42% | 0.18 | |
| SiO2 | 53.40% | 2.47 | |
| Oxide Weight | 274.33 | ||
| Formula Weight | 274.33 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |