General Frit GF-143

Alternate Names: Frit 143, Frit GF143

Description: Sodium Boron Silicate Leadless

Oxide Analysis Formula Tolerance
Na2O 8.48% 1.00
B2O3 38.48% 4.04
SiO2 53.04% 6.45
Oxide Weight 731.13
Formula Weight 731.13

Notes

A 'specific-oxide' borosilicate frit (contains only sodium, boron, silica).
Used to bond abrasives.

Related Information

Links

Materials Ferro Frit 3185
Materials Fusion Frit F-245
Materials Ferro Frit 3226
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Fusion Frit F-367
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 6.40
Frit Softening Point 1750F