General Frit GF-115

Alternate Names: Frit 115, Frit GF115

Description: High Calcium Boron Leadless for partially-fritted tile glazes

Oxide Analysis Formula Tolerance
CaO 11.43% 0.68
Na2O 5.95% 0.32
B2O3 23.15% 1.11
Al2O3 11.92% 0.39
SiO2 47.55% 2.64
Oxide Weight 333.65
Formula Weight 333.65

Related Information

Links

Materials Fusion Frit F-2
Materials F-2 Ball Clay
Materials Ferro Frit 3195
A commonly used boron frit, it is a balanced glaze all along at cone 06-02 (with the addition of 10-15% kaolin). Not fully glossy.
Materials Pemco Frit P-67
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 6.90
Frit Softening Point 1800F