Fusion Frit F-125

Alternate Names: Fusion Frit F125

Description: Wall Tile Opaque Frit

Oxide Analysis Formula Tolerance
CaO 7.00% 0.39
K2O 2.00% 0.07
Na2O 10.90% 0.55
ZrO2 15.00% 0.38
B2O3 21.50% 0.96
SiO2 43.60% 2.25
Oxide Weight 310.74
Formula Weight 310.74

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit CZ-105
Materials Pemco Frit P-3V126
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 7.01
Frit Softening Point 1500F