Pemco Frit P-3V126

Alternate Names: 3V126,3V-126

Description: Opaque tile frit

Related Information

Links

Oxide Analysis Formula Tolerance
Materials Fusion Frit F-125
Materials Ferro Frit CZ-105
Materials General Frit GF-126
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.