Degussa Frit 90198

Description: Leadless high alkali borosilicate frit

Oxide Analysis Formula Tolerance
K2O 17.70% 0.50
Na2O 11.65% 0.50
B2O3 26.16% 1.00
Al2O3 3.83% 0.10
SiO2 40.66% 1.80
Oxide Weight 266.10
Formula Weight 266.10

Related Information

Links

Materials Frit 6004
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.