1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Frit 6004

Alternate Names: Frit VO6004p

Description: Israel

Oxide Analysis Formula Tolerance
K2O 15.50% 0.47
Na2O 11.50% 0.53
B2O3 25.50% 1.05
Al2O3 3.50% 0.10
SiO2 44.00% 2.09
Oxide Weight 285.69
Formula Weight 285.69

Related Information

Links

Materials Degussa Frit 90198
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy