Hommel Frit 3GF61A

Description: LEADLESS FRIT

Oxide Analysis Formula Tolerance
BaO 2.56% 0.07
CaO 7.89% 0.61
K2O 3.75% 0.17
MgO 0.49% 0.05
Na2O 1.12% 0.08
SrO 0.27% 0.01
B2O3 16.88% 1.05
Al2O3 10.92% 0.47
SiO2 56.12% 4.06
Oxide Weight 434.82
Formula Weight 434.82

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.