Ferro Frit 3466

Description: Low lead, low boron, low alumina glaze frit cone 2-7

Oxide Analysis Formula Tolerance
BaO 1.50% 0.03
CaO 7.10% 0.42
K2O 1.40% 0.05
Na2O 2.70% 0.14
PbO 17.70% 0.26
ZnO 2.40% 0.10
B2O3 5.60% 0.27
Al2O3 8.90% 0.29
SiO2 52.70% 2.89
Oxide Weight 329.45
Formula Weight 329.45

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Fusion Frit FZ-23
Materials Hommel Frit 581
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 7.2
Frit Melting Range (C) 1500F