Monthly Tech-Tip from Tony Hansen SignUp

No tracking! No ads!

1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Ferro Frit 3463

Oxide Analysis Formula Tolerance
BaO 0.03% -
CaO 0.42% 0.01
K2O 0.05% -
Na2O 0.14% -
PbO 0.26% -
ZnO 96.00% 0.99
B2O3 0.27% -
Al2O3 0.29% -
SiO2 2.89% 0.04
Oxide Weight 84.25
Formula Weight 84.25

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.