Ferro Frit 3458

Description: Low lead calcium borate frit

Oxide Analysis Formula Tolerance
BaO 1.40% 0.03
CaO 7.01% 0.46
K2O 1.44% 0.06
Na2O 2.65% 0.16
PbO 17.70% 0.29
B2O3 5.31% 0.28
Al2O3 9.33% 0.34
SiO2 55.17% 3.38
Oxide Weight 368.47
Formula Weight 368.47

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 7.1
Frit Melting Range (C) 1500F