Ferro Frit 3447

Description: Barium lead calcuim borosilicate frit

Oxide Analysis Formula Tolerance
BaO 23.34% 0.26
CaO 10.30% 0.31
K2O 5.48% 0.10
Na2O 4.72% 0.13
PbO 25.99% 0.20
B2O3 7.79% 0.19
Al2O3 16.45% 0.27
SiO2 5.92% 0.17
Oxide Weight 170.46
Formula Weight 170.46

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Hommel Frit 2GF65E
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 7.6 x 10-6
Frit Melting Range (C) 1600F