Ferro Frit 3403

Description: Lead alumina bisilicate frit

Oxide Analysis Formula Tolerance
CaO 0.10% 0.01
K2O 1.40% 0.05
Na2O 0.30% 0.01
PbO 67.80% 0.93
Al2O3 2.30% 0.07
SiO2 28.10% 1.44
Oxide Weight 307.46
Formula Weight 307.46

Notes

Cone Range: 08-02
This is basically a lead bisilicate frit with a few impurities.
Very low melting temperature.

Related Information

Links

Materials Fusion Frit FL-42
Materials Pemco Frit Pb-723
Materials General Frit GF-9
Materials Ferro Frit 3602
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Hommel Frit 437
Materials Lead Bisilicate Frit
A standard frit of 1 molar part of PbO and 2 of SiO2. It is considered stable and non-leachable.
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 7.2
Frit Melting Range (C) 1350F
By Tony Hansen