1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Ferro Frit 3230

Description: Very high alkaline frit for copper blue, manganese purples

Oxide Analysis Formula Tolerance
BaO 2.04% 0.03
K2O 11.11% 0.25
Na2O 18.92% 0.64
ZnO 3.21% 0.08
SiO2 64.72% 2.26
Oxide Weight 210.13
Formula Weight 210.13

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Mechanisms

Glaze ColorFrits with very high alkali and little or no alumina can develop these colors well. However they have very high thermal expansion so it is difficult to get them to fit most bodies.
Glaze ColorFrits with very high alkali and little or no alumina can develop these colors well. However they have very high thermal expansion so it is difficult to get them to fit most bodies.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy