1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Alkatrol W-20031

Oxide Analysis Formula Tolerance
K2O 1.30% 0.07
Na2O 1.30% 0.10
TiO2 0.51% 0.03
Al2O3 21.00% 1.00
SiO2 73.09% 5.91
Fe2O3 0.41% 0.01
LOI 2.40%n/a
Oxide Weight 474.11
Formula Weight 485.76

Notes

This version has higher alklai (and therefore lower PCE), coarser particle size, higher specific gravity and bulk density.

Related Information

Links

Materials Alkatrol W-22535
Materials Alkatrol
Typecodes Aluminum Silicate
Materials not classifiable as commonly known aluminum silicates. For example, kaolin is a common aluminum silicate.

Data

Pyrometric Cone Equivalent 16

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy