1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Alkatrol W-22535

Oxide Analysis Formula Tolerance
K2O 0.65% 0.04
Na2O 0.65% 0.05
TiO2 0.40% 0.03
Al2O3 20.00% 1.00
SiO2 75.90% 6.44
Fe2O3 0.40% 0.01
LOI 2.00%n/a
Oxide Weight 499.80
Formula Weight 510.00

Notes

This version has lower alklai (and therefore higher PCE), finer particle size, lower specific gravity and bulk density.

Related Information

Links

Materials Alkatrol W-20031
Materials Alkatrol
Typecodes Aluminum Silicate
Materials not classifiable as commonly known aluminum silicates. For example, kaolin is a common aluminum silicate.

Data

Pyrometric Cone Equivalent 19

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy