Error: API server returned an invalid response for materialDescription: Leadless alkali borosilicate frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.20% | 0.01 | |
| K2O | 4.13% | 0.17 | |
| Na2O | 12.60% | 0.81 | |
| B2O3 | 26.12% | 1.50 | |
| Al2O3 | 17.66% | 0.69 | |
| SiO2 | 39.29% | 2.61 | |
| Oxide Weight | 398.99 | ||
| Formula Weight | 398.99 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Materials |
Ferro Frit 3227
|
| Materials |
Fusion Frit F-395
|
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 5.80 |
|---|---|
| Co-efficient of Linear Expansion | 9.4 |
| Frit Melting Range (C) | 1450F |