Alternate Names: F3227 Frit, F3227
Description: Low melting bonding frit used in metals industry
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| K2O | 4.10% | 0.16 | |
| Na2O | 13.90% | 0.84 | |
| B2O3 | 28.50% | 1.53 | |
| Al2O3 | 15.60% | 0.57 | |
| SiO2 | 37.90% | 2.36 | |
| Oxide Weight | 373.53 | ||
| Formula Weight | 373.53 | ||
| Materials |
Fusion Frit F-395
|
| Materials |
Ferro Frit 90 742 F
|
| Materials |
Ferro Frit 90 741 F
|
| Materials |
Ferro Frit 3221
|
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Typecodes |
Bonding Frits
Also called glass frits, these melt at very low temperatures (e.g. 500C). They are used to bond together materials that can withstand some heat (e.g. abrasives, ceramics, non-oxide ceramics, metals). And as a surface-smoothing agent. The main product properties are melting temperature and thermal expansion. The powders are mixed with binders, applied and then heated up and down to create the bond. |
| Co-efficient of Linear Expansion | 9.8 |
|---|---|
| Frit Melting Range (C) | 1300F |