1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Colorobia Frit 621

Description: Barium frit

Oxide Analysis Formula Tolerance
SiO2 57.30% 3.87
Al2O3 11.40% 0.45
Fe2O3 0.30% 0.01
TiO2 0.10% 0.01
CaO 7.00% 0.51
MgO 0.50% 0.05
Na2O 3.70% 0.24
K2O 1.20% 0.05
ZrO2 0.25% 0.01
ZnO 0.20% 0.01
PbO 0.20% -
SrO 0.20% 0.01
B2O3 11.30% 0.66
BaO 4.80% 0.13
Oxide Weight 399.89
Formula Weight 399.89