Alternate Names: KaoPearl, CNL30
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Fe2O3 | 0.60% | 0.01 | |
| K2O | 1.30% | 0.04 | +/- 0.25 |
| SiO2 | 47.50% | 2.18 | |
| Al2O3 | 37.00% | 1.00 | |
| TiO2 | 0.05% | - | |
| Na2O | 0.15% | 0.01 | |
| CaO | 0.05% | - | |
| MgO | 0.30% | 0.02 | |
| Oxide Weight | 239.70 | ||
| Formula Weight | 239.70 | ||
An Imerys product, apparently a possible replacement for Super Standard Porcelain. Available in North America. The data sheet indicates a production site in Cornwall, UK. Their first data sheet was released in March 2021.
The K2O varies somewhat.
| Materials |
Super Standard Porcelain
|
| Materials |
Grolleg Kaolin
A white burning kaolin from the UK, commonly used in porcelain bodies and as a glaze suspender. Sticky when wet, low plasticity. |
| Typecodes |
Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content. |
| URLs |
https://digitalfire.com/4sight/datasheets/KaoPearlCNL30.pdf
KaoPearl CNL30 Data Sheet Release date: March 2021 |
| By Tony Hansen Follow me on ![]() | ![]() |
Buy me a coffee and we can talk