Description: Ancienne fritte
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| BaO | 2.73% | 0.05 | |
| CaO | 10.94% | 0.53 | |
| MgO | 0.40% | 0.03 | |
| K2O | 1.50% | 0.04 | |
| Na2O | 8.22% | 0.36 | |
| Al2O3 | 6.48% | 0.17 | |
| B2O3 | 16.21% | 0.63 | |
| SiO2 | 53.52% | 2.40 | |
| Oxide Weight | 269.36 | ||
| Formula Weight | 269.36 | ||
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |