Torrecid Frit MBK00020

Description: Calcium zinc zircon zero boron matte frit

Oxide Analysis Formula Tolerance
ZnO 4.38% 0.14
Al2O3 18.56% 0.47
ZrO2 9.50% 0.20
MgO 2.12% 0.13
Na2O 2.08% 0.09
SiO2 46.56% 1.98
K2O 2.69% 0.07
Fe2O3 0.13% -
CaO 12.46% 0.57
TiO2 1.39% 0.04
LOI 3.34%n/a
Oxide Weight 255.67
Formula Weight 264.50

Notes

Soft surface, high opacity. Used for the new decoration technology: Inkjet

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy