Torrecid Frit MBK00007

Description: Zinc calcia magnesia titania low-alumina zero-boron frit

Oxide Analysis Formula Tolerance
ZnO 11.96% 0.29
MgO 4.03% 0.20
Al2O3 3.03% 0.06
Fe2O3 0.15% -
CaO 12.74% 0.45
SiO2 54.12% 1.78
Na2O 0.30% 0.01
TiO2 5.40% 0.13
K2O 2.68% 0.06
ZrO2 4.30% 0.07
SO4 1.29%n/a
Oxide Weight 194.57
Formula Weight 197.12

Notes

Matte, soft surface. High opacity. Affected by chemical attack.
Multicolor surface effects (likely due to high titanium content).

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.