Esmalglass Frit FO 940/1

Oxide Analysis Formula Tolerance
SrO 0.10% -
K2O 1.10% 0.02
Na2O 1.00% 0.03
SiO2 46.00% 1.27
BaO 0.20% -
Fe2O3 0.10% -
CaO 20.10% 0.59
ZnO 0.50% 0.01
MgO 8.40% 0.35
ZrO2 0.40% 0.01
Al2O3 19.80% 0.32
LOI 0.60%n/a
Oxide Weight 162.04
Formula Weight 163.02

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Frit Softening Point 910C
Frit Melting Range (C) 1245C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy