Esmalglass Frit FT 8547

Alternate Names: Esmalglass Frit 8547

Oxide Analysis Formula Tolerance
P2O5 0.10% -
K2O 5.40% 0.12
Fe2O3 0.10% -
Na2O 0.90% 0.03
Al2O3 7.50% 0.16
SiO2 60.50% 2.16
MgO 1.20% 0.06
CaO 14.90% 0.57
ZnO 7.90% 0.21
BaO 0.10% -
LOI 0.60%n/a
Oxide Weight 211.76
Formula Weight 213.04

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Frit Softening Point 1090C
Frit Melting Range (C) 1170C