Frit 37.062

Alternate Names: Frit 37 062, Frit 37-062

Oxide Analysis Formula Tolerance
CaO 8.42% 0.36
BaO 29.60% 0.46
K2O 5.73% 0.15
MgO 0.58% 0.03
Al2O3 5.83% 0.14
ZrO2 2.64% 0.05
B2O3 4.23% 0.15
SiO2 42.97% 1.71
Oxide Weight 239.01
Formula Weight 239.01

Related Information

Data

Frit Melting Range (C) 980-1060C