Ferro Richoux Frit 21 C005

Description: Fritte Alcaline

Oxide Analysis Formula Tolerance
K2O 10.18% 0.21
Na2O 18.51% 0.58
CaO 3.03% 0.10
BaO 8.29% 0.11
Al2O3 4.88% 0.09
B2O3 3.76% 0.10
SiO2 51.35% 1.66
Oxide Weight 194.29
Formula Weight 194.29

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Frit Melting Range (C) 880-1060C