Frit VO 6160

Description: Reimbold & Strick fast firing Zn,Ba matte frit

Oxide Analysis Formula Tolerance
CaO 3.00% 0.12
K2O 1.00% 0.02
ZrO2 11.00% 0.20
Na2O 3.00% 0.11
MgO 1.00% 0.06
BaO 18.00% 0.27
ZnO 15.00% 0.42
Al2O3 7.00% 0.16
B2O3 5.00% 0.16
SiO2 36.00% 1.36
Oxide Weight 227.80
Formula Weight 227.80

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 56 x 10-7 (20-400C)
Frit Softening Point 660C
Glass Transition Temperature 600C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy