Frit VO 6086

Description: Reimbold & Strick barium matte frit

Oxide Analysis Formula Tolerance
Al2O3 12.00% 0.36
CaO 5.00% 0.27
SiO2 51.00% 2.60
BaO 25.00% 0.50
K2O 7.00% 0.23
Oxide Weight 306.26
Formula Weight 306.26

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
URLs http://www.reimbold-und-strick.de/images/pdf/keramisch.pdf
Reimbold & Strick Frit chart with chemistry

Data

Co-efficient of Linear Expansion 67 x 10-7 (20-400C)
Frit Softening Point >800C
Glass Transition Temperature 660C