Frit A 3323

Description: Reimbold & Strick stoneware opaque frit

Oxide Analysis Formula Tolerance
SiO2 52.00% 3.43
K2O 2.00% 0.08
MgO 2.00% 0.20
Na2O 6.00% 0.38
ZrO2 9.00% 0.29
CaO 4.00% 0.28
BaO 2.00% 0.05
Al2O3 9.00% 0.35
B2O3 14.00% 0.80
Oxide Weight 396.86
Formula Weight 396.86

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
URLs http://www.reimbold-und-strick.de/images/pdf/keramisch.pdf
Reimbold & Strick Frit chart with chemistry

Data

Co-efficient of Linear Expansion 58 x 10-7 (20-400C)
Frit Softening Point 640C
Glass Transition Temperature 560C