Solargil Frit FR11

Description: Barium frit

Oxide Analysis Formula Tolerance
BaO 4.95% 0.27
CaO 4.83% 0.72
B2O3 22.04% 2.65
K2O 0.11% 0.01
SiO2 56.37% 7.85
Al2O3 11.70% 0.96
Oxide Weight 836.44
Formula Weight 836.44

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.