Error: API server returned an invalid response for material

Ferro Frit CC-279-3 (approx)

Alternate Names: Frit CC-279

Description: Fluorine lithium strontium zircon borate frit

Oxide Analysis Formula Tolerance
Li2O 2.50% 0.19 2.5
F 2.50% 0.30 2.5
SiO2 52.50% 2.01 2.5
B2O3 17.50% 0.58 2.5
Na2O 7.50% 0.28 2.5
K2O 5.00% 0.12 2.5
CaO 7.50% 0.31 2.5
MgO 0.50% 0.03 .5
SrO 2.50% 0.06 2.5
Al2O3 7.50% 0.17 2.5
ZnO 0.50% 0.01 .5
ZrO2 0.50% 0.01 2.5
Oxide Weight 245.22
Formula Weight 245.22

Notes

This is a USA pottery frit. Lagunaclay.com sells it in small quantities as of 2019. They claim this to be a "Cone 07-06 all-fritted glossy glazes."

Ferro only publishes an approximate analysis, that is shown here.
This is for fritted or highly fritted clear glazes.

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
Typecodes Available from Laguna Clays
URLs https://digitalfire.com/4sight/datasheets/ferropotteryfrits2008.pdf
Ferro Pottery Frits 2008

Data

Co-efficient of Linear Expansion 8.32 x 10-6

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy